  1. Misruns
  2. Shrinkage cavity
  3. Cold shuts
  4. Cold shots

Answer (Detailed Solution Below)

Option 1 : Misruns
Free
Intelligence Test Battery Practice Set 1 (Easy to Moderate)
2.6 K Users
35 Questions 35 Marks 10 Mins

Detailed Solution

Download Solution PDF

Explanation:

Casting defects

Cold Shut

  • A cold shut is caused when two streams while meeting in the mould cavity, do not fuse together properly thus forming a discontinuity in the casting.
  • When the molten metal is poured into the mould cavity through a more-than-one gate, multiple liquid fronts will have to flow together and become one solid.

Misrun:

  • When the molten metal solidifies before completely filling the mold cavity and leaves a space in the mold called as misrun.
  • Cause:
    • Low fluidity of the molten metal.
    • Low temperature of the molten metal which decreases its fluidity.
    • Too thin section and improper gating system.

F1 Krupalu 14.1.21 Pallavi D3

Shrinkage Cavities:
  • It is a void on the surface of the casting caused mainly due to uncontrolled and haphazard solidification of the metal. 
  • These are caused by the liquid shrinkage occurring during the solidification of the casting. 
  • To compensate this, proper feeding of liquid metal is required and also proper casting design. 
  • Shrinkage defects can be split into two different types: 
    • Open shrinkage defects
    • Closed shrinkage defects

F5 Tabrez 14-1-2021 Swati D1

Latest DFCCIL Executive Updates

Last updated on Jul 7, 2025

-> DFCCIL admit card 2025 for Executives has been released at the official website.

-> DFCCIL Executive exam date 2025 has been released. DFCCIL exam date is July 10 & 11.

-> DFCCIL Executive city intimation slip has been released. 

->  DFCCIL Executive Recruitment 2025 Correction window is open from 31st March, to 4th April 2025.

-> Candidates can make corrections in their application form, if they have made any mistake. There will be 100/- fee for correction in form.

-> DFCCIL Executive Recruitment 2025 application deadline has been extended.

-> Eligible and Interested candidates had applied from 18th January 2025 to 22nd March 2025.  

-> A total of 175 Vacancies have been announced for multiple posts like Executive (Civil, Electrical, Signal and Telecommunication).

-> Candidates who will get a successful selection under the DFCCIL Recruitment 2025 for the Executive selection process will get a salary range between Rs. 30,000 to Rs. 1,20,000.

-> Candidates must refer to the DFCCIL Executive Previous Year Papers to prepare well for the exam.

Get Free Access Now
Hot Links: teen patti boss teen patti master gold download teen patti stars teen patti comfun card online teen patti flush