When two distinct metals in an electrolyte come in contact with one another, it results in galvanic corrosion. Ions, which are atoms or group of atoms that have gained or lost electrons, are present in the electrolyte solution. The ions in the electrolyte might transfer from one metal to the other when two different metals come into contact with one another. The two metals may corrode or wear away as a result of this. Anodic corrosion is the most typical kind of galvanic corrosion. Anodic corrosion is when one metal corrodes more quickly than the other because it is more active or has a greater electrode potential. The more energetic metal will become more positive as a result of losing electrons. The metal that is less active will turn more adverse. Until they reach a condition of equilibrium, where the rate of corrosion is the same for both metals, the two metals will keep corroding.
In this Chemistry, we will learn about Galvanic corrosion in detail:
Galvanic corrosion is a method in which one metal corrodes more quickly than another when it comes into contact with an electrolyte, also referred to as bimetallic corrosion. When two different metals are electrically linked and submerged in a conductive fluid, galvanic corrosion happens. The anode is corroded, whereas one metal (the cathode) is protected. Compared to the rate when the metal is uncoupled, the rate of attack on the anode is accelerated.
Only in the presence of an electrolyte that may provide a route for the movement of ions and an electric conducting path between the metals does galvanic corrosion take place.
Get 5 Days SuperCoaching @ just
₹329₹329
These are the examples of galvanic corrosion:
When zinc and copper metals are submerged in an electrolyte, which might be water or an aqueous solution containing any salt, like copper sulphate and the circuit is complete.
Until the zinc electrode is entirely dissolved, the procedure is repeated. Hydrogen gas, which appears as bubbles near the cathode, is also produced from the electrolyte's hydrogen ions.
Due to its larger oxidation potential than the cathode, zinc now starts to oxidise. Zinc starts to corrode as a result, producing zinc ions. On the other hand, copper ions start to pick up electrons and decrease, safeguarding the metal.
This is the mechanism of galvanic corrosion:
These are the causes of galvanic corrosion:
The potential difference between the two metals in a galvanic cell is what makes it functional. This potential difference is what causes the movement of electrons inside the cell. A metal electrode's ability to oxidise and lose electrons is known as its oxidation potential. The metal may release its electrons more readily the greater the oxidation potential. The oxidation potential has the exact opposite magnetic field as the reduction potential. It is the ability of a metal ion to absorb electrons and undergo reduction in solution. The oxidation potential of metals is used to build an electrochemical series.
There are three major causes of galvanic corrosion:
An increased danger of electron loss results from the faster oxidation of the elements at the top of the series. Two metal electrodes are placed in an electrolyte to start the corrosion process, and a wire is then used to complete the circuit. Whereas metals with a lower oxidation potential will start acting as cathodes and gaining electrons, those with a higher oxidation potential will start acting as anodes and losing electrons.
Galvanic corrosion occurs when two metals are dipped in a container full of liquid, they come in contact with each other and are electrically coupled. The higher electrode potential metal will corrode more quickly in an electrochemical cell formed by the two metals.
Galvanic corrosion is caused by a number of factors, including:
These are the preventions of galvanic corrosion:
Now learning is easy and fun for the students with the Testbook app. This app is specially curated for students preparing for national entrance examinations. It has notes curated by the experts and mock tests which are developed while keeping the nature of the examination. It is available on both iOS and Android versions of the phone. Download your Testbook App from here now, and get discounts on your first purchase order.
Download the Testbook APP & Get Pass Pro Max FREE for 7 Days
Download the testbook app and unlock advanced analytics.